Week 8 LAB: The Experiment Explained

The Experiment, Explained in Plain English
Shakera Karolia · BioClub Tokyo · 17 November 2026
A companion to the Week 8 LAB experimental proposal. The proposal is written for a reviewer who already knows the field. This document is written for anyone — it explains what the experiment actually is, how it answers the assignment, and why each decision was made rather than some other one.
1 — The experiment in one paragraph
I am growing the same bacterium, in the same food, in two different kinds of plastic cup, and measuring two things: how much bacterial film grows in each, and — more importantly — how similar the answer is from one cup to the next.
That is genuinely the whole experiment. Everything else in this document explains why that simple comparison is worth running, and why each small decision inside it was made the way it was.
2 — What the assignment asked, and what I had to decide
The Week 8 lab is a single experiment run across the whole course. Everyone grows the same organism by the same method. Each participant chooses one thing to change, explains why, and the results are pooled.
There were two choices available:
| Option | What it means |
|---|---|
| Vary the medium | Change something in the liquid food — sugar, salts, a mineral, a supplement |
| Vary the substrate | Change the surface the film grows on |
The rule is that you change one and hold the other completely fixed. That constraint is not bureaucratic; it is the entire point, and §6 explains why.
I chose the substrate. The rest of this document is the reasoning.
3 — Why the course is growing a biofilm on purpose
This is worth understanding first, because it explains why consistency matters more than quantity in everything that follows.
A biofilm is what bacteria build when they stop swimming around and settle on a surface. They stick down and secrete a slime layer around themselves. The familiar example is dental plaque; the clinically serious examples are infections on catheters, joint replacements, heart valves and in the lungs of people with cystic fibrosis.
Biofilms matter because they are extraordinarily hard to kill. A bacterium floating freely is easy to destroy with an antibiotic. The same bacterium inside a biofilm can survive doses hundreds of times higher — not because it has evolved resistance, but because the slime blocks the drug from reaching it and the cells deep inside go dormant.
So researchers need to test new treatments against biofilms rather than against free-floating bacteria. And to do that, they need a biofilm they can make the same way twice.
Here is the problem the course exists to solve:
Suppose you test two different treatments against two batches of biofilm, and one treatment works better. You want to conclude that the treatment is better. But if your two biofilm batches were not the same to begin with, you cannot. The difference might be in the treatment — or it might just be in the biofilm.
Published biofilm work varies so much between batches that this is a real and frequent problem. The course is therefore trying to manufacture a biofilm to a specification, the way a factory manufactures anything else — so that every batch is interchangeable and any difference you see afterwards genuinely comes from the treatment you applied.
This is why my experiment measures consistency, not just quantity. A surface that grows lots of biofilm but a different amount every time is worse, for this purpose, than a surface that grows less but grows it reliably.
4 — Why I chose the surface rather than the food
Most participants changed something in the food. I changed the surface, for a reason specific to this particular bacterium.
The organism is Mycobacterium smegmatis — a harmless soil relative of the bacterium that causes tuberculosis. It is used because it is safe to handle but shares the unusual feature that makes its dangerous relatives so hard to treat.
That feature is its outer surface. Most bacteria have a fairly ordinary outer coat. Mycobacteria are wrapped in mycolic acids — extremely long, greasy, fatty molecules. In practical terms, the outside of this bacterium is waxy. That waxiness is why mycobacteria clump together into rope-like bundles, and a large part of why tuberculosis is so difficult to cure.
Two published findings make this more than a curiosity:
- The bacterium actively rebuilds that greasy coat while it is forming a biofilm. It is not a passive feature; it is part of the process. Strains that cannot build it properly fail to form biofilms properly (Ojha et al., 2005).
- The same greasiness is what drives the cells to clump and stick in the first place (DePas et al., 2019).
So here is the logic:
If the sticky part of the bacterium is grease, then the property of the surface that should matter most is how greasy or how watery that surface is.
In technical terms that property is surface free energy, and it is measured as the contact angle — how much a water droplet beads up on the surface rather than spreading out.
Nobody else was testing that. Several people were testing different materials — plastic versus metal versus glass. But swapping plastic for titanium changes four things at once: the chemistry, the stiffness, the roughness and the wettability. If you see a difference, you cannot say which of the four caused it.
So I kept the material identical and changed only its surface finish. Same plastic, two different top coatings. That isolates exactly one property.
5 — The two surfaces, and why those two specifically

Figure 1 — The two surfaces. On the left, water beads up on untreated plastic — a water-repellent surface, which the waxy bacterium should like. On the right, water spreads flat on the coated plastic — a water-attracting surface engineered to resist things sticking to it.
Both plates are polystyrene, the ordinary clear plastic that laboratory plates are made from. The difference is only in the outermost few nanometres:
| S-HI — the reference | S-LO — the test | |
|---|---|---|
| What it is | Plain, untreated plastic | Plastic with a bonded “ultra-low attachment” hydrogel coating |
| Water behaviour | Beads up (water-repellent) | Spreads flat (water-attracting) |
| Electrical charge | Uncharged | Neutral |
| Protein sticking | Protein sticks readily | Engineered to resist protein sticking |
Why not the obvious comparison?
The obvious experiment is untreated plastic versus tissue-culture-treated plastic — those are the two plate types every lab already has on the shelf.
I deliberately did not do that, and this is the single most important decision in the design.
The manufacturer’s own documentation gives three facts:
- untreated plastic is water-repellent and uncharged
- tissue-culture-treated plastic is water-attracting and negatively charged
- the hydrogel coating is water-attracting and neutrally charged
Look at the first two carefully. Going from untreated to tissue-culture-treated changes two things at once — the wettability and the electrical charge. If you then see a difference in biofilm, you cannot say which one caused it. You are back to the same problem as swapping plastic for titanium, just more subtly.
The hydrogel coating solves this. It is water-attracting like the tissue-culture plate, but neutral, like the untreated plate. So between my two arms, the charge stays effectively unchanged and only the wettability moves.

Figure 2 — Why this pairing and not the usual one. Think of the two properties as two axes. The conventional comparison moves diagonally — both properties change together, so the result is ambiguous. My comparison moves straight across — only wettability changes, so whatever difference appears can be attributed to it.
In plain terms: if you want to find out whether sugar makes coffee sweeter, you do not add sugar and milk at the same time. The conventional plate comparison adds sugar and milk. Mine adds only sugar.
One further benefit worth noting: because the untreated plate is the common starting point for both comparisons, my experiment and the conventional one add together rather than overlapping. If an untreated-versus-tissue-culture dataset exists elsewhere in the programme, the charge effect that neither experiment measures directly can be worked out by subtraction, since both are measured against the same reference.
5b — “Why not just drop a disc in the well?”
This is the fairest criticism of my design, so I want to answer it head-on.
The brief says the substrate is “something you place in the 96 well plate.” Most people did exactly that — they cut a small disc of their material and dropped one into each well. I didn’t. I changed the whole plate.
Doing it with discs would have been better in two ways. Both of my surfaces could sit in one single plate, which would remove the only real weakness in my design (see §6). And it would be cheaper and easier for the lab running it.
So I tried to design the disc version. It doesn’t work. Here is why, because the reason turns out to be interesting in itself.

Figure 7 — Four ways to make a disc version, and why each one fails.
The problem is that “wettable” and “negatively charged” come as a package
If you want to make plastic water-attracting, the standard method is to blast it with plasma — an energised gas that chemically bolts oxygen-containing groups onto the surface. Those groups are what make it wettable.
They are also what make it negatively charged.
So you cannot use plasma to change wettability on its own. You get both, always. That is precisely the confound I designed my experiment to avoid — I’d have walked straight back into it.
Glass has the same problem from the other direction. Bare glass is water-attracting but carries a negative charge; coat it to make it water-repellent and the charge disappears too. Same package deal.
And on rubbery materials, the treatment doesn’t even stay put
There’s a second, separate problem if you try this on silicone — the soft rubber that catheters and drains are made of.
Plasma-treating silicone works, but it wears off. Molecules from deep inside the material slowly migrate up to the surface and undo the treatment. This is called hydrophobic recovery, and it happens over hours to days.
My experiment runs for three to five days.

Figure 8 — The surface has to hold still while the biofilm grows. The shaded band is when I harvest. A plasma-treated silicone surface is still changing throughout it — so the thing I claim to be testing would be sliding around while the bacteria were responding to it. The hydrogel coating stays flat because it is chemically bonded on, not just energised on.
There’s a twist worth noting. Of ten polymers tracked for over 100 days in one study, polystyrene held its treatment the longest. So a plasma-treated polystyrene disc would actually be stable enough. But polystyrene is exactly the material where plasma gives you the negative charge — so you buy stability and pay for it with the confound. There is no free option.
What I chose, and what it cost me
The hydrogel coating is the only surface I found that is water-attracting, electrically neutral, and chemically bonded so it doesn’t drift. It solves both problems at once.
It is only sold as a complete plate. You cannot buy it as a disc.
So I took the trade: I accepted a known, manageable weakness — two plates instead of one — in order to get the only version of this experiment where the thing I’m measuring actually stays still and means one thing.
The principle: when you can’t meet a specification, say which constraint is binding and what you traded for it. Don’t quietly swap in a different experiment that looks like it satisfies the brief but no longer answers the question.
6 — What is held constant, and why that is the real work

Figure 3 — One thing changes; everything else is pinned. The list on the left is not padding. Each item is a thing that could otherwise explain a difference between the two arms, and each one is deliberately eliminated.
This is the part that looks like fussiness and is actually the experiment.
An experiment can only tell you that A caused B if A is the only thing that was different. Every item on that list is a thing that, if allowed to vary, could produce a difference between my two plates that had nothing to do with the surface.
A concrete example: if I made the medium on Monday for one plate and on Wednesday for the other, and the Wednesday batch happened to be slightly different, I would see a difference between the plates and wrongly attribute it to the surface. So: one batch of medium, both plates, same day.
The same reasoning applies to the inoculum, the volumes, the temperature, the humidity, the incubation time and the incubator position.
Two specific decisions worth explaining
Why the iron level is fixed at a particular value, not just “some iron.” Iron is known to matter for this organism specifically — published work shows that this bacterium needs supplemental iron to form a mature biofilm, although it does not need it to grow normally while floating free. Iron is therefore an active variable for the exact process I am studying. Leaving it unspecified would leave a known lever loose. I pinned it at the protocol’s own standard reference level, which also means my results sit on the same baseline as everyone else’s and can be compared directly.
Why the replicate wells are scattered rather than grouped. Wells around the edge of a plate behave differently from wells in the middle — they lose more liquid to evaporation and sit at a slightly different temperature. This is a well-documented effect. If I put all my replicates together in one block, that block’s position would quietly bias every one of them in the same direction. Scattering them randomly across the plate means the edge effect averages out instead of accumulating. The outer ring of wells is filled with plain water, which raises the humidity inside the plate and reduces the evaporation in the first place.
The one thing I could not fully eliminate, stated openly
The two surfaces come as two separate plates. That means “which surface” and “which plate” are tangled together — in principle, a difference could come from the plate rather than the coating.
Participants testing different materials avoid this by cutting small discs and dropping them into wells of one single plate. I cannot do that, because surface treatment is only sold as a whole plate; you cannot buy a disc of it.
So instead of ignoring the problem, I control it: both plates get the same medium batch, the same culture, the same day, the same incubator run, with positions rotated. That removes every realistic route by which “which plate” could produce a difference. The proposal states this limitation explicitly rather than hiding it.
7 — What actually happens, step by step

Figure 4 — The procedure, with the reason for each step. Steps 1, 2 and 5 exist to remove alternative explanations. Step 4’s blank wells exist to separate the plate’s own signal from the biofilm’s. Step 7 is where the actual answer is produced.
In words:
- One batch of medium is made, enough for every well on both plates. One batch, so the food cannot differ between arms.
- One culture of the bacterium is grown and adjusted to a standard density. The detergent used during growth is washed off, because detergent would interfere with sticking — which is the thing being measured.
- Two plates are laid out, one of each surface. Replicate wells are scattered; the outer ring is filled with water.
- Cells and medium are added to a fixed volume of 200 µL per well. Some wells get medium but no cells — these are the blanks, and §8 explains why they matter so much.
- Both plates are incubated together for three to five days, in the same run, with positions rotated.
- The biofilm is stained with crystal violet, a purple dye that sticks to biofilm. Unbound dye is washed away, the bound dye is dissolved, and the colour intensity is read by a machine. More colour means more biofilm.
- The blank is subtracted and the final numbers are calculated: the average for each surface, and the consistency score for each surface.
8 — How it is measured, and the trap built into the measurement
Crystal violet is the standard biofilm stain. It is a positively charged purple dye, and it sticks to negatively charged material — which biofilm is.
Here is the trap, and it is specific to my experiment.
My two surfaces have different chemistry. A positively charged dye will not necessarily stick to them equally even when there is no biofilm there at all. So some of the purple I measure may be the plate, not the bacteria. And because the two plates differ, the amount of “plate purple” may differ too.
If I ignored that, I could get a completely wrong answer — not just an imprecise one, but one pointing in the wrong direction.

Figure 5 — Why the blank wells are essential. Each surface has its own empty-well control, processed through exactly the same staining steps. Only the difference is reported. If the two blanks differ in size and are not each subtracted from their own surface, the comparison can be compressed, erased, or reversed.
So the rule in my protocol is strict: every surface gets its own blank wells, run through the complete staining procedure, and the reported number is always the biofilm reading minus that surface’s own blank. The blank values are published alongside the results rather than quietly removed, so anyone can check the correction.
The two numbers that come out
| Number | What it is | What it tells you |
|---|---|---|
| Mean | Average corrected reading for each surface | How much biofilm that surface grows |
| CV | How spread out the replicates are, as a percentage | How reliably that surface grows it |
CV — coefficient of variation — is just the spread divided by the average. A low CV means every well came out roughly the same. A high CV means they scattered.
CV is the answer I actually care about. The mean supports it.
9 — What I predict, and why
Prediction 1 — how much biofilm
Less biofilm on the coated surface than on the plain one.
The reasoning is the greasiness argument from §4: a waxy bacterium should stick well to a water-repellent surface and badly to a water-attracting one that is specifically designed to resist things sticking.
Why this is worth knowing beyond the immediate result: it tests whether you can stop this bacterium from attaching using surface chemistry alone — no antibiotic, no disinfectant, nothing released into the surroundings. That matters practically, because medical device manufacturers cannot easily change what their devices are made of, but they can and do apply coatings. If a plain, neutral coating meaningfully reduces attachment, that is a real-world intervention and not just a laboratory observation.
Prediction 2 — how consistent, which is the one that matters
Lower CV (better consistency) on the plain untreated surface.
This prediction is my own reasoning, not something taken from a paper, and the proposal labels it as such.
The argument runs like this. Whether a biofilm starts in a given well is a bit like whether a seed takes root. On a surface the bacteria stick to easily, essentially every cell that lands stays put — so every well gets a similar start, and the wells end up similar. On a surface they barely stick to at all, whether any given well gets going becomes closer to a coin flip — so the wells scatter. There is also a simple arithmetic effect: as the average falls towards zero, the percentage spread rises, because you are dividing by a smaller and smaller number.

Figure 6 — The consistency prediction, and the honest limit of a two-point experiment. The solid line is what this experiment can test: consistency improves as stickiness increases. The dashed line is a fuller version of the same idea — that consistency is worst in the middle, where sticking is borderline. Two points cannot tell those two shapes apart. Distinguishing them would need a third surface in between, and the figure says so rather than pretending otherwise.
Why this prediction is interesting rather than obvious: if it holds, the recommendation to the programme is slightly perverse. It says use the plain, boring, untreated plate — not because it is better biology, but because it is the more reliable manufacturing process. At this stage of the project, a dependable result beats a dramatic one.
10 — What each possible outcome would mean
A well-designed experiment is one where every outcome teaches you something. Here is what each result would mean, decided in advance so the interpretation cannot drift to fit the data.

Figure 7 — The three outcomes, and what each one says.
Outcome A — the surfaces differ. Wettability drives attachment, as predicted. The straightforward result.
Outcome B — the surfaces come out the same. This would look like a failure, and is not one.
The medium contains broken-down protein as a nutrient. Protein sticks to water-repellent surfaces within minutes — much faster than bacteria attach. So it is quite possible that the bacteria never touch my plastic at all; they may touch a thin protein film that formed on it first. If that film covers both surfaces equally, both plates behave identically and the surface stops mattering.

Figure 8 — The protein film, and why this pairing resists it. Protein piles onto the water-repellent surface but is actively repelled by the hydrogel coating, which is engineered for exactly that. This is a second, independent reason for choosing the hydrogel as the test surface — it is the one most likely to stay distinguishable even if a film forms.
If both arms converge anyway, the correct conclusion is that the medium, not the plate, defines the surface the bacteria actually experience. That is a genuinely useful finding: it tells the whole programme to stop worrying about plates and start worrying about medium composition. It can be tested directly by adding a condition where the plate is soaked in sterile medium for an hour first, then inoculated.
Outcome C — the coated surface shows almost nothing. If attachment is suppressed nearly completely, the reading sits down at the blank and the consistency score becomes mathematically unstable — you cannot meaningfully compute a percentage spread around a number that is essentially zero. In that case the result is reported as a detection limit: “attachment was suppressed below what this assay can measure,” rather than a misleading ratio. Deciding this in advance stops it from becoming an awkward judgement call later.
11 — How this connects back to the assignment
The assignment asked for one variable and a rationale. Here is the chain, start to finish:
| Step | Decision | Why |
|---|---|---|
| 1 | Vary the substrate, not the medium | The medium space was well covered; the surface property the organism’s own biology points at was not being tested |
| 2 | Vary surface treatment, not material | Changing material changes four properties at once and cannot attribute an effect |
| 3 | Use untreated vs neutral hydrogel, not untreated vs tissue-culture | The conventional pairing changes wettability and charge together; this pairing changes only wettability |
| 4 | Hold everything else fixed, in one batch, on one day | So that nothing except the surface can explain a difference |
| 5 | Use surface-matched blanks | Because the dye is charged and the surfaces differ, so part of the signal is the plate itself |
| 6 | Report consistency as the headline, biomass as support | Because the programme’s goal is a reproducible test article, not a large one |
| 7 | Pre-commit to the meaning of every outcome | So the interpretation cannot be adjusted after seeing the data |
And the quiet point underneath the whole thing:
The shared protocol says “standard 96-well flat-bottom polystyrene.” Untreated and tissue-culture-treated plates both fit that description. They look identical, sit next to each other in the storeroom, and get swapped without anyone writing it down. If different sites are using different boxes, then plate surface is an uncontrolled factor sitting underneath everyone’s results — including all the medium experiments, none of which would show any sign of it.
My experiment measures how big that hidden factor is. And it produces something you can act on: a plate catalogue number plus a measurable acceptance check, which is the sort of thing you can put on a purchase order and verify when the box arrives. That is what it takes to manufacture anything to a specification.
12 — Plain-English glossary
| Term | In plain English |
|---|---|
| Biofilm | A layer of bacteria stuck to a surface inside slime they make themselves. Dental plaque is one. |
| Blank | A well with everything except bacteria, used to measure what the plate alone contributes to the reading. |
| Casamino acids | Broken-down milk protein used as bacterial food. Its protein fragments cause the “protein film” complication. |
| Contact angle (θ) | How much a water droplet beads up on a surface. High angle = water-repellent. Low angle = water-attracting. |
| Cording | The rope-like clumping of mycobacteria, caused by their greasy outer coat. |
| Crystal violet | A purple dye that sticks to biofilm. Standard way to measure how much biofilm is there. |
| CV (coefficient of variation) | Spread divided by average, as a percentage. Low CV = consistent. High CV = scattered. |
| Detection limit | The smallest amount the test can reliably distinguish from nothing. |
| Edge effect | Wells on the outside of a plate behave differently because they evaporate more and sit at a different temperature. |
| Hydrogel coating (ULA) | A bonded, water-attracting, electrically neutral coating designed to stop things sticking. |
| Hydrophobic / hydrophilic | Water-repellent / water-attracting. |
| Hydrophobic recovery | When a plasma treatment wears off and a surface slowly goes back to being water-repellent, over hours to days. |
| Inoculum | The starting dose of bacteria added to each well. |
| Insert / disc | A small piece of test material dropped into a well. The way most people varied the substrate. |
| PDMS / silicone | The soft rubber used for catheters, drains and tubing. |
| Plasma treatment | Blasting a surface with an energised gas to make it water-attracting — which also makes it negatively charged. |
| Mycolic acids | The very long, greasy fatty molecules that make up the mycobacterial outer coat. |
| OD₆₀₀ | A cloudiness measurement used to judge how many bacteria are in a liquid culture. |
| Planktonic | Floating freely, as opposed to stuck to a surface. |
| Polystyrene | The clear plastic laboratory plates are made of. |
| Replicate | A repeat of the same condition. Comparing replicates is how consistency is measured. |
| Substrate | The surface the biofilm grows on. |
| Surface free energy | The physical property that determines whether things wet and stick to a surface. Measured as contact angle. |
| Tissue-culture-treated | Plastic that has been chemically modified to be water-attracting — but which also becomes negatively charged in the process. |
| ΔOD₅₉₀ | The final reported number: the colour reading with that surface’s own blank subtracted. |
13 — Sources for the factual claims
DePas WH, Bergkessel M, Newman DK (2019). Aggregation of nontuberculous mycobacteria is regulated by carbon–nitrogen balance. mBio 10(4):e01715-19. https://doi.org/10.1128/mBio.01715-19 — the greasy envelope and its role in clumping
Ojha A, Anand M, Bhatt A, Kremer L, Jacobs WR, Hatfull GF (2005). GroEL1: a dedicated chaperone involved in mycolic acid biosynthesis during biofilm formation in mycobacteria. Cell 123(5):861–73. https://doi.org/10.1016/j.cell.2005.09.012 — the bacterium actively rebuilds its greasy coat while forming a biofilm
Ojha A, Hatfull GF (2007). The role of iron in Mycobacterium smegmatis biofilm formation. Molecular Microbiology 66(2):468–83. https://doi.org/10.1111/j.1365-2958.2007.05935.x — iron is needed for biofilm but not for ordinary growth
Corning Life Sciences. Corning Surfaces for Cell Culture, CLS-CC-013. https://www.corning.com/catalog/cls/documents/product-information-sheets/CLS-CC-013.pdf — the charge and wettability of each plate surface
Corning Life Sciences. Corning Ultra-Low Attachment Surface. https://www.corning.com/worldwide/en/products/life-sciences/products/surfaces/ultra-low-attachment-surface.html — the hydrogel coating is neutral, water-attracting, and resists protein
Jokinen V, Suvanto P, Franssila S (2012). Oxygen and nitrogen plasma hydrophilization and hydrophobic recovery of polymers. Biomicrofluidics 6(1):016501. https://doi.org/10.1063/1.3673251 — ten polymers tracked for 100+ days; polystyrene held its treatment longest
Hydrophobic recovery of PDMS surfaces in contact with hydrophilic entities (2022). Materials 15(6):2313. https://doi.org/10.3390/ma15062313 — silicone recovers over hours to days
14 — What in here is mine
The published findings above are cited and are not my work. The following are my own reasoning:
- the argument that how water-attracting a surface is — rather than what it is made of — is the property matched to a greasy bacterial coat;
- the choice of a neutral water-attracting surface instead of the conventional one, specifically so that charge does not change alongside wettability;
- the observation that this makes my comparison and the conventional one add together through their shared reference rather than overlap;
- the prediction that consistency is better on the stickier surface, and the counter-intuitive recommendation that follows from it;
- the identification of differing dye retention between the two surfaces as a trap requiring surface-matched blanks;
- the point that plate surface may be an unrecorded variable sitting underneath other results in the programme;
- the decision to report near-total suppression as a detection limit rather than as a ratio;
- the elimination of the disc-format alternatives in §5b, and the point that every way of making a surface water-attracting by oxidation also makes it negatively charged — the argument is mine, the recovery behaviour it rests on is cited.
All diagrams are original and were drawn for this submission. Figures 5 and 6 are illustrative and do not show real data. Contact angle values are supplier specifications to be verified, not measurements I have taken.
End of document.